ʻO ka copolymer butadiene-styrene i hoʻopau ʻia me ka rubber-hydroxyl wai (HTBS)

Wehewehe Pōkole:

ʻO HTBS kahi copolymer wai o ka butadiene a me ka styrene me ka hui hana hydroxyl ma ka hopena o ke kaulahao molekala, he kūpaʻa wela maikaʻi loa ia, kūpaʻa abrasion, kūpaʻa ʻelemakule, hana hana maikaʻi, hanauna wela haʻahaʻa a me ka maʻalahi o ka mahana haʻahaʻa maikaʻi.


Nā kikoʻī huahana

Nā nīnau i nīnau pinepine ʻia

Nā Lepili Huahana

Nā Waiwai a me nā Hoʻohana

ʻO HTBS kahi copolymer wai o ka butadiene a me ka styrene me ka hui hana hydroxyl ma ka hopena o ke kaulahao molekala, he kūpaʻa wela maikaʻi loa ia, kūpaʻa abrasion, kūpaʻa ʻelemakule, hana hana maikaʻi, hanauna wela haʻahaʻa a me ka maʻalahi o ka mahana haʻahaʻa maikaʻi.

Hiki ke hoʻohana ʻia me ka laholio kūlohelohe a me ka laholio synthetic, a hiki ke hoʻohana wale ʻia no ka hoʻolei ʻana i nā kaila polyurethane, ka mea hoʻopili ipu, ka mea hoʻopili, a pēlā aku. Loaʻa iā ia ka hana traction maikaʻi loa a me ke kūpaʻa i ka abrasion ke hoʻohana ʻia i ka laholio hehi.

Nā kikoʻī loea

Helu Huahana.

HTBS2000

HTBS3000

HTBS4000

Helu awelika kaumaha molekala

1800-2200

2700-3300

3600-4400

Ka waiwai hydroxyl, mmol/g

0.8-1.2

0.6-0.8

0.45-0.55

Ka nui o ka styrene (wt.%)

15-25

15-25

15-25

Ka mānoanoa (25 ℃, Pa-s)

≤12

≤20

≤80

Mea lele (%)

≤0.50

helehelena

Wai mānoanoa melemele māmā